Hydrogen Embrittlement Behavior on Microalloyed Pipeline Steel in NS-4 Solution

N/A
N/A
Protected

Academic year: 2019

Share "Hydrogen Embrittlement Behavior on Microalloyed Pipeline Steel in NS-4 Solution"

Copied!
17
0
0

Loading.... (view fulltext now)

Full text

Figure

Figure 1.  Microalloyed Pipeline Steel Plate Microstructure. a) Optical and b) SEM microphotographies
Figure 2.  Electrochemical corrosion steel behavior in NS-4 test solution, (a)polarization curves and (b)  EIS Nyquist plot
Figure 3.  Microalloyed steel slow and fast sweep rates under NS-4 solution
Figure 4.  (if-is)/is values from the slow and fast sweep rates related to different polarization curves potentials