• No results found

High wear resistance

Wear Resistance of Industrial Pure Iron Treated by Nitriding and Quenching Followed by Aging Process

Wear Resistance of Industrial Pure Iron Treated by Nitriding and Quenching Followed by Aging Process

... The wear resistance of iron nitrides compound layers and a high nitrogen martensite phase formed in the material surface for industrial pure iron, treated by nitriding and quenching followed by aging ...

6

Effect of mating materials on wear properties of amorphous hydrogenated carbon (a-C:H) coating and tetrahedral amorphous carbon (ta-C) coating in base oil boundary lubrication condition

Effect of mating materials on wear properties of amorphous hydrogenated carbon (a-C:H) coating and tetrahedral amorphous carbon (ta-C) coating in base oil boundary lubrication condition

... as high hardness, low friction and high wear resistance (Kano, 2006; Erdemir and Donnet, ...and wear properties of DLC-mating tribopairs (Topolovec-Miklozic et ...the wear ...

20

Effect of destabilization treatment on microstructure, hardness and abrasive wear of high chromium hardfacing

Effect of destabilization treatment on microstructure, hardness and abrasive wear of high chromium hardfacing

... erosion resistance are required. Th e high wear resistance of high chromium hardfacing is attributed to the combination of hard primary and/or eutectic car- bides of M 7 C 3 (M – metal: ...

8

An Experimental Investigation into Wear Resistance of Mg-SiC Nanocomposite Produced at High Rate of Compaction

An Experimental Investigation into Wear Resistance of Mg-SiC Nanocomposite Produced at High Rate of Compaction

... The high wear resistance of Mg-SiC samples produced by SHPB can be attributed to its increased hardness and also to the strong bonding between the nanoreinforcement and Mg matrix that facilitates the ...

11

Cold spray deposition of thermoplastic powder for road marking

Cold spray deposition of thermoplastic powder for road marking

... with high wear resistance, increased service life, which can be used in various climatic zones in the temperature range from -40 °C to +40 °C, which will allow replacing water and solvent based ...

5

Structure and tribological properties of post-sputtered annealing nickel titanium alloy coatings onto 316l stainless steel.

Structure and tribological properties of post-sputtered annealing nickel titanium alloy coatings onto 316l stainless steel.

... higher wear resistance of NiTi compared with many tribological ...The wear resistance of conventional tribo-materials strongly depends on their mechanical properties such as hardness, ...

26

A Review Paper on Research and Analysis of Non Asbestos Composite Material

A Review Paper on Research and Analysis of Non Asbestos Composite Material

... their high strength to weight ratio, low cost and high wear resistance are widely manufactured and used in structural applications along with aerospace, high temp applications, circuit ...

10

Wear Resistance of Steels with Surface Nanocrystalline Structure Generated by Mechanical Pulse Treatment

Wear Resistance of Steels with Surface Nanocrystalline Structure Generated by Mechanical Pulse Treatment

... of high wear resistance, a special atten- tion has been paid to steels with nanocrystalline struc- ture (NCS) which have a complex, unique mechanical properties ...combine high characteristics ...

5

GRADIENT COMPOSITE COATINGS FOR WORKING SURFACES OF BRAKING DEVICES

GRADIENT COMPOSITE COATINGS FOR WORKING SURFACES OF BRAKING DEVICES

... with high wear resistance and working in by forming its gradient structure: a thin surface layer of dispersed structure with low shear resistance and depth of the columnar structure oriented ...

5

Effects of Electron Beam Irradiation on Impact Value of Carbon Fiber Reinforced Thermoplastic Polyetheretherketone

Effects of Electron Beam Irradiation on Impact Value of Carbon Fiber Reinforced Thermoplastic Polyetheretherketone

... On the other hand, the homogeneous low voltage electron beam irradiation (HLEBI) often induces not only the hard- ening, high wear resistance and sterilization for practical use of polymer, but also ...

7

Modification of Friction Knots Work Surfaces on the Basis of Microarc Oxidation Method

Modification of Friction Knots Work Surfaces on the Basis of Microarc Oxidation Method

... However, as have shown further investigations, the growth of the cathode discharges, unlike from anodic ones, in most cases without organization of special conditions does not lead to formation of quality coatings with ...

17

Preparation And Mechanical Behaviour Of Al-6063-Sicp Aluminum Matrix Composites By Using Stir Casting Technique

Preparation And Mechanical Behaviour Of Al-6063-Sicp Aluminum Matrix Composites By Using Stir Casting Technique

... The elastic limit of any material is the point at which it can no longer return to its original shape or size. The elastic limit determined by a torsion test is equal to the slope of the line from the start of testing ...

12

Evaluation on Microstructure and Mechanical Behaviour of Al6061 Al2O3 Gr Hybrid Composites

Evaluation on Microstructure and Mechanical Behaviour of Al6061 Al2O3 Gr Hybrid Composites

... In recent scenario, it was found that, among all the aluminium alloys, Al6061 is (popular) admired as matrix material system in development of MMC’s owing to its good corrosion resistance and excellent mechanical ...

15

Si DLC coatings optimized for low wear and low friction applications

Si DLC coatings optimized for low wear and low friction applications

... based wear protective films were deposited on polycarbonate by a special arc plasma torch starting from oxygen and organosiloxane [111] ...and high-frequency PECVD for the deposition of silicon-based ...

181

Betterment of life of the cutting tool by process of heat treatment

Betterment of life of the cutting tool by process of heat treatment

... One can notice that while measuring out of tool life of a material, it is needed maintain constant feed and depth of cut for all cutting tool materials. However, there is a fluctuation shall takes place only for speed of ...

5

Improvement of High Temperature Wear Resistance of AISI 316 ASS through NiCrBSiCFe Plasma Spray Coating

Improvement of High Temperature Wear Resistance of AISI 316 ASS through NiCrBSiCFe Plasma Spray Coating

... adhesive wear (seizure) conditions result in formation of 20 to 40µm thick layer with the fine-crystalline microstructure ...coating wear and friction ...the wear resistance and the friction ...

18

STUDY OF WEAR BEHAVIOUR OF Al/ (Al2O3P and SiCP) HYBRID METAL MATRIX COMPOSITES

STUDY OF WEAR BEHAVIOUR OF Al/ (Al2O3P and SiCP) HYBRID METAL MATRIX COMPOSITES

... sliding wear behaviour of Aluminium Hybrid Metal Matrix Composite was investigated and a prediction model was developed using Taguchi’s ...the wear properties was evaluated. It was found that as load ...

11

Engine oil wear resistance

Engine oil wear resistance

... Viscosity of oil plays a vital role in selecting a lubricant because correct lubricant will help to maximize engine life. Society of Automotive Engineers (SAE) has developed viscosity classification to engine oils to ...

11

Survey on Cladding Low Carbon Steel with Nickel Based Alloys by using GMAW Process

Survey on Cladding Low Carbon Steel with Nickel Based Alloys by using GMAW Process

... M.H. Amushahi [4] et al, demonstrates hard- facing of low carbon steel using a boron-rich cored wire electrode. Boride-rich cored wires have found wide industrial applications in cladding and hard surfacing, especially ...

5

Impact of cryogenic cooling during machining: A Literature Review

Impact of cryogenic cooling during machining: A Literature Review

... Abstract- Evolution in new engineering materials like difficult to cut materials, super alloys & composites materials and following of strict international norms during machining the use of conventional cutting ...

6

Show all 10000 documents...