nickel base superalloy
Effect of Hot Isostatic Pressing on Microstructure and Mechanical Properties of CM 681LC Nickel Base Superalloy Using Microcast
9
Fatigue Behavior and Life Prediction Model of a Nickel Base Superalloy under Different Strain Conditions
8
Submicron Structure of Rhenium Base Diffusion Barrier Coating Layer on a Nickel Base Superalloy
5
Impact of forging direction on the recrystallization behaviour of nickel base superalloy AD730 billet material at subsolvus temperatures
33
Influence of Rhenium on the Grain Boundary Strength, Phase Evolution, and High Temperature Mechanical Properties of a Fine Grain Nickel Base Superalloy at 982°C
9
Transmission Electron Microscopy Sample Preparation of INCONEL 738 Nickel-Base Superalloy
8
Research on Interlayer Alloys for Transient Liquid Phase Diffusion Bonding of Single Crystal Nickel Base Superalloy DD6
9
Detection of Rhenium Rich Particles at Grain Boundaries in Nickel Base Superalloy Turbine Blades
9
Influence of the initial cooling rate from γ′ supersolvus temperatures on microstructure and phase compositions in a nickel superalloy
41
Effect of strain level on the evolution of microstructure in a recently developed AD730 nickel based superalloy during hot forging
21
Low cycle fatigue of a directionally solidified Nickel based superalloy : testing, characterisation and modelling
12
Cyclic oxidation behavior of uncoated and aluminum-rich nickel aluminide coated Rene-80 superalloy
7
μ Phase in a Nickel Base Directionally Solidified Alloy
5
A nickel(II) complex of an unsymmetrical tetradentate Schiff base
15
Experimental Study and Computer Simulation of Fracture Toughness of Ni Base Superalloy using CT Specimen
13
Effects of Rhenium on Microstructure and Phase Stability of MAR M247 Ni Base Fine Grain Superalloy
8
Modelling plastic deformation in a single-crystal nickel-based superalloy using discrete dislocation dynamics
14
Hydrothermal synthesis of copper (II) and Nickel (II) nano complexes with unsymmetric tetradentate Schiff base ligand. New precursors for preparation of copper (II) and nickel (II) oxides nano-particles
8
Elemental preference and atomic scale site recognition in a Co Al W base superalloy
6
Fatigue crack growth in a Nickel based superalloy at elevated temperature : experimental studies, viscoplasticity modelling and XFEM predictions
14